BÖHLER M261
BÖHLER M261
- Polishability 40%
- Thermal conductivity 40%
- Wear resistance 40%
- Toughness 80%
- Machinability 80%
Designations
-
6 Side Processing
-
Flat Plate
-
Gun Drilling
-
Saw Cutting Flat Plate
-
Surface Grinding
Chemical composition
C | 0.13 | Si | 0.30 | Mn | 2.00 |
S | 0.15 | Cr | 0.35 | Ni | 3.50 |
Cu | 1.20 | Al | 1.20 |